The bevel gear is the most common intersecting-shaft transmission component in gearboxes, differentials and machine tool indexing mechanisms. Once the geometry has been calculated, the next step must be the strength verification — both the tooth flank contact fatigue strength and the root bending fatigue strength have to pass. If either fails, flank pitting, tooth breakage and tooth fracture will follow one after another, and the whole machine grinds to a halt.
The following works through one complete example, taking the two steps of tooth flank contact and root bending verification from start to finish, then explains the formula system.
A pair of straight bevel gears: shaft angle Σ = 90°, pinion tooth count z1 = 20, gear tooth count z2 = 40, module m = 4 mm, face width b = 30 mm, transmitted power P = 7.5 kW, pinion speed n1 = 1450 r/min, pinion material 40Cr quenched and tempered, flank hardness 280 HBW, gear material C45 steel quenched and tempered, flank hardness 240 HBW, unidirectional operation, smooth load, service life 10 years (300 working days per year, 16 h per day).
Transmission ratio i = z2/z1 = 40/20 = 2
Pitch cone angle δ1 = arctan(z1/z2) = arctan(20/40) = arctan(0.5) = 26.565°
Pitch cone angle δ2 = 90° − δ1 = 63.435°
Pinion pitch circle d1 = m·z1 = 4×20 = 80 mm
Gear pitch circle d2 = m·z2 = 4×40 = 160 mm
Cone distance R = 0.5·d1/sin δ1 = 40/sin 26.565° = 40/0.4472 = 89.44 mm
Equivalent tooth count zv1 = z1/cos δ1 = 20/0.8944 = 22.36
Equivalent tooth count zv2 = z2/cos δ2 = 40/0.4472 = 89.44
Pinion torque T1 = 9550·P/n1 = 9550×7.5/1450 = 49.40 N·m
Circumferential force at the pinion pitch circle Ft1 = 2T1/d1 = 2×49400/80 = 1235 N
Pitch circle at the face width midpoint dm1 = d1 − b·sin δ1 = 80 − 30×0.4472 = 66.58 mm
Midpoint circumferential force Ftm = 2T1/dm1 = 2×49400/66.58 = 1484 N
Application factor KA = 1.00 (smooth load, uniform motor drive)
Dynamic factor Kv = 1.05 (accuracy grade 7, circumferential velocity v = π·dm1·n1/(60×1000) = π×66.58×1450/60000 ≈ 5.05 m/s, from the table)
Tooth flank load sharing factor KHα = 1.2 (straight bevel gear, non-uniform load distribution along the tooth)
Tooth flank load distribution factor KHβ = 1.15 (medium rigidity housing)
Total load factor K = KA·Kv·KHα·KHβ = 1.00×1.05×1.2×1.15 = 1.449
The contact fatigue strength verification formula (per the Mechanical Design Handbook for straight bevel gears):
σH = ZE·ZH·√(K·Ftm·(√(u²+1)) / (dm1·b·0.85)) ≤ [σH]
where u = z2/z1 = 2; the face width coefficient 0.85 is the equivalent face width coefficient for straight bevel gears
Elastic coefficient ZE = 189.8 √MPa (steel on steel)
Zone coefficient ZH = √(2cosβ·cosαt/(sinαt·cosαt)) ≈ 2.5 (straight teeth β=0, αt=20°)
Calculating the contact stress:
σH = 189.8 × 2.5 × √(1.449×1484×√(4+1) / (66.58×30×0.85))
= 474.5 × √(1.449×1484×2.236 / 1698.79)
= 474.5 × √(4806.6 / 1698.79)
= 474.5 × √2.829 = 474.5 × 1.682 = 798 MPa
Look up the permissible contact stress [σH]: 40Cr quenched and tempered 280 HBW, [σH] = 680 MPa (converted for a 10-year life)
σH = 798 MPa > [σH] = 680 MPa, the contact strength does not pass!
Verification conclusion: the module must be increased from 4 to 5, or an alloy steel with carburizing and quenching adopted (the permissible contact stress can reach 1100 MPa).
The root bending strength verification formula:
σF = (K·Ftm·YFa·YSa·Yε) / (b·mm) ≤ [σF]
Mean module mm = m·(R − 0.5b)/R = 4×(89.44−15)/89.44 = 4×0.832 = 3.328 mm
Tooth form coefficient YFa1 = 2.97 (zv1 = 22.36, interpolated from the table)
Stress correction coefficient YSa1 = 1.52
Tooth form coefficient YFa2 = 2.45 (zv2 = 89.44)
Stress correction coefficient YSa2 = 1.62
Contact ratio coefficient Yε = 0.85 (approximate value)
Root bending stress of the pinion:
σF1 = (1.449×1484×2.97×1.52×0.85) / (30×3.328) = 8268 / 99.84 = 82.8 MPa
Root bending stress of the gear (larger lever arm, fewer teeth in contact):
σF2 = σF1·(YFa2·YSa2) / (YFa1·YSa1) = 82.8×(2.45×1.62)/(2.97×1.52) = 82.8×2.55 = 138.6 MPa
Look up the permissible bending stress [σF]: 40Cr quenched and tempered, [σF]1 = 320 MPa; C45 steel quenched and tempered, [σF]2 = 230 MPa
σF1 = 82.8 MPa < 320 MPa ✓
σF2 = 138.6 MPa < 230 MPa ✓, the bending strength passes!
Verification conclusion: the bending strength margin is ample, so the critical link is contact fatigue.
| Verification item | Calculated stress | Permissible stress | Result |
|---|---|---|---|
| Tooth flank contact fatigue | 798 MPa | 680 MPa | ❌ does not pass |
| Pinion root bending | 82.8 MPa | 320 MPa | ✓ passes |
| Gear root bending | 138.6 MPa | 230 MPa | ✓ passes |
Improvement scheme: increase the module m from 4 to 5, or use 20CrMnTi with carburizing and quenching (permissible contact stress 1100 MPa).
Tooth flank contact fatigue failure appears as flank pitting and spalling, and is caused by the cyclic contact stress on the flank exceeding the contact fatigue limit of the material. It is the main failure mode of a closed drive with soft tooth flanks (flank hardness ≤ 350 HBW).
Root bending fatigue failure appears as tooth fracture, and is caused by the maximum root bending stress exceeding the bending fatigue limit of the material. It is the main failure mode of open gear drives and hard flank gears (flank hardness > 350 HBW).
Unlike a spur gear, two points require special treatment in the strength calculation of a bevel gear:
The design is qualified when the calculated stress σ ≤ the permissible stress [σ], and unqualified otherwise. If either of the two verifications fails, that failure mode is the weak link of the design and must be specifically improved (increase the module, change the material, increase the face width, reduce the load, and so on).
| Parameter | Meaning | How to obtain the value |
|---|---|---|
| ZE | Elastic coefficient | Steel on steel 189.8 √MPa; steel on cast iron 165.4 √MPa |
| ZH | Zone coefficient | ≈ 2.5 for straight teeth; varies with the helix angle for helical teeth |
| u | Tooth ratio | u = z2/z1 |
| dm1 | Pinion midpoint pitch circle | dm1 = d1 − b·sin δ1 |
| Ftm | Midpoint circumferential force | Ftm = 2T1/dm1 |
| K | Total load factor | K = KA·Kv·KHα·KHβ |
| [σH] | Permissible contact stress | Look up in the handbook table, converted for the required life |
| Parameter | Meaning | How to obtain the value |
|---|---|---|
| YFa | Tooth form coefficient | Look up by zv = z/cos δ |
| YSa | Stress correction coefficient | Look up by zv |
| Yε | Contact ratio coefficient | Generally taken as 0.85 |
| mm | Mean module | mm = m·(R−0.5b)/R |
| [σF] | Permissible bending stress | Look up by material + tooth direction + life |
The contact stress formula for a helical bevel gear (βm ≠ 0) must be multiplied by the helix angle coefficient Zβ:
For βm = 35°, Zβ ≈ 1.16; the midpoint pitch circle dm1 is calculated with the normal module mn to obtain the equivalent value.
| Transmitted power P | Pinion speed n1 | Recommended module m |
|---|---|---|
| ≤ 3 kW | ≤ 1500 r/min | 2~3 mm |
| 3~10 kW | 1000~2000 r/min | 3~5 mm |
| 10~30 kW | 800~1500 r/min | 5~8 mm |
| 30~75 kW | 500~1000 r/min | 8~12 mm |
| ≥ 75 kW | ≤ 800 r/min | ≥ 12 mm |
| Support condition | Recommended φR |
|---|---|
| Overhung at both ends | 0.20~0.25 |
| Simply supported (bearings at both ends) | 0.25~0.30 |
| Crossed mounting (high rigidity) | 0.30~0.35 |
Above 0.35 the tooth thickness at the small end is too thin and the strength is insufficient; below 0.20 the face width is too narrow and the load capacity is poor.
| Material | Heat treatment | Hardness | [σH] | [σF] |
|---|---|---|---|---|
| C45 steel | Quenched and tempered | 220~250 HBW | 560~600 MPa | 200~230 MPa |
| 40Cr | Quenched and tempered | 260~280 HBW | 650~700 MPa | 280~320 MPa |
| 35SiMn | Quenched and tempered | 220~260 HBW | 620~680 MPa | 240~280 MPa |
| 20CrMnTi | Carburized and quenched | 58~62 HRC | 1050~1200 MPa | 320~380 MPa |
| 38CrMoAl | Nitrided | ≥ 850 HV | 1100~1250 MPa | 300~360 MPa |
| No. | Common mistake | Consequence | Correct practice |
|---|---|---|---|
| 1 | Forgetting to multiply by 0.85 (the equivalent face width coefficient) in the contact stress formula | The verification result is unsafe, and the actual contact stress is higher | Strictly follow the formula: dm1·b·0.85 (straight bevel gears) |
| 2 | Substituting the large-end pitch circle d1 directly into the calculation | The contact stress comes out too small and the strength is wrongly judged as passing | The midpoint pitch circle dm1 = d1 − b·sin δ1 must be used |
| 3 | Looking up the tooth form coefficient by z (without dividing by cos δ) | The bending stress calculation is wrong | Look up YFa and YSa by the equivalent tooth count zv = z/cos δ |
| 4 | Using the basic permissible stress directly without converting it for the required life | Too conservative for short-life designs, and dangerously non-conservative for long-life designs | [σ] = σlim·ZN/S; a life coefficient correction is mandatory for long-life designs |
| 5 | Verifying only the pinion and ignoring the gear bending stress | The gear (larger z but a larger force per tooth) may break first | Verify both gears and take the larger bending stress |
| 6 | Ignoring KHα and KHβ (taking K=1 directly) | The effect of the uneven load distribution is underestimated | Look up the four Ki coefficients from the table according to the duty condition |
To summarize: the key to bevel gear strength verification lies in the two core concepts of the "midpoint section" and the "equivalent tooth count". The contact strength depends mainly on the module and the material hardness, while the bending strength depends mainly on the tooth form (the equivalent tooth count). For closed drives look at contact, for open drives look at bending — this is the universal rule of gear selection. In the next issue we cover the transmission ratio distribution of a multi-stage gear reducer, explaining the optimization of multi-stage distribution thoroughly in one go.