Phosphor bronze CuSn6 (GB QSn6.5-0.1) · Tin-phosphor bronze

Chemical composition per GB/T 5231 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.

Chemical composition (mass fraction %)

Sn6.0~7.0
P0.10~0.25
Cubalance

Mechanical properties (typical values)

ConditionTensile MPaYield MPaElong. %Hardness
M temperapprox. 350~450——approx. 70~90HB
Y temperapprox. 500~650——approx. 150~200HB

Heat treatment

Not heat-treatable for strengthening; used in work-hardened tempers.

Typical applications

Elastic elements (diaphragms/spring strips), sliding bearings, worm wheels, and screw nuts. Wear-resistant + elastic + anti-magnetic.

Selection tips & common mistakes

Related materials

Brass CuZn39 (GB H62) Aluminium bronze CuAl9Fe4 (GB QA19-4)

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL