Strength and uses of brass, bronze and cast copper alloys for wear parts, conductive parts and worm-wheel pairing materials.
| Grade | Condition | sigma_b (MPa) ref. | Typical use |
|---|---|---|---|
| H62 | Annealed | ≥294 | Gaskets, conduits, stamped parts |
| HPb59-1 | Annealed | ≥343 | Machined parts: valve cores, nuts (free-cutting brass) |
| QSn6.5-0.1 | Hard | 470~640 | Spring elements, wear strips (tin bronze) |
| QAl9-4 | — | ≥540 | High-strength wear parts, worm wheels |
| ZCuSn10P1 | Metal-mold cast | ≥310 | Worm-wheel rim, plain bearing (with steel worm) |
| ZCuAl10Fe3 | Sand cast | ≥490 | Heavy-duty worm wheels, nuts, bearings |
Worm-wheel rims use tin bronze for low friction and wear; paired with a steel worm it gives the lowest friction coefficient. Aluminum bronze is stronger but slightly less antifriction. Copper is costly – substitute steel + surface treatment where possible.
See all quick calculators on the knowledge base home page.
Data compiled from publicly available GB/T standard tables for design reference only. For final design and acceptance, always consult the original standard and the latest supplier catalog.