Chemical composition per GB/T 11352 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | ≤0.40 |
| Si | ≤0.50 |
| Mn | ≤0.90 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Normalized + tempered | ≥500 | ≥270 | ≥18 | ≥22J (impact) |
Supplied normalized + tempered (or Q&T). Grade reading = σb/σs, same style as the Q235 system.
Parts of complex shape requiring more toughness than cast iron: frames, rocker arms, lifting lugs, wagon connectors.
Ductile iron QT450-10 (EN-GJS-450-10) ZG310-570 cast carbon steel (high-strength)