The cylinder barrel is the “skeleton” of a hydraulic cylinder — it carries the entire working pressure. If the wall is too thin it bulges or even bursts; if it is too thick it is heavy, expensive and space-consuming. The core of getting the wall thickness right is “first calculate the allowable stress, then decide thin or thick wall, then round off and confirm”. Below we run through this procedure with a 25 MPa medium-to-high-pressure cylinder.
Bore D = 100 mm, working pressure p = 25 MPa, material C45 steel quenched and tempered, yield strength σs = 360 MPa, static safety factor n = 2.5.
Find: the barrel wall thickness δ and the outer diameter D₁.
Safety factor: 2~2.5 for static load, 3~4 for dynamic load. Taking 2.5 for a medium-to-high-pressure cylinder already leaves ample margin.
The thin-wall formula applies only to medium and low pressure thin-wall cylinders with D/δ ≥ 10. It is simple and quick, so use it for the first estimate.
Above 10 means a thin wall and the formula is reliable. Below 10 means a thick wall, and the fourth strength theory thick-wall formula must be used.
Here D/δ is close to 10 (the borderline), so check with the thick-wall formula: 8.76 mm is close to the 8.68 mm from the thin-wall formula, and both methods are reliable.
Take the standard wall thickness of 10 mm and an outer diameter of 120 mm. Rounding the wall thickness up to a standard value settles the barrel parameters.
| Type | Criterion | Formula used | Applicable |
|---|---|---|---|
| Thin-wall cylinder | D/δ ≥ 10 | δ = pD/(2[σ]) | Medium and low pressure cylinders (p ≤ 16 MPa) |
| Thick-wall cylinder | D/δ < 10 | The fourth strength theory thick-wall formula | High / ultra-high pressure cylinders (p > 16 MPa) |
| Material | Heat treatment | σs (MPa) | Recommended pressure |
|---|---|---|---|
| 20 steel | Normalising | 245 | ≤ 7 MPa low pressure |
| C45 steel | Quenched and tempered | 360 | ≤ 25 MPa medium pressure |
| 27SiMn | Quenched and tempered | 835 | ≤ 31.5 MPa high pressure |
| 35CrMo | Quenched and tempered | 835+ | Ultra-high pressure |
1. Allowable stress:
2. Thin-wall formula:
3. Thick-wall formula (fourth strength theory):
4. Outer diameter:
5. Thin wall / thick wall criterion:
| Symbol | Meaning | Unit | Value notes |
|---|---|---|---|
| D | Bore diameter | mm | From the GB/T 2348 standard |
| p | Working pressure | MPa | 1 MPa = 1 N/mm² |
| δ | Wall thickness | mm | Round up to a standard value |
| σs | Yield strength of the material | MPa | Look it up by material grade |
| n | Safety factor | — | 2~2.5 for static load, 3~4 for dynamic load |
| Duty condition | Safety factor n | Notes |
|---|---|---|
| Static load | 2.0~2.5 | Steady pressure with no shock |
| Ordinary dynamic load | 3.0~4.0 | With pressure pulsation |
| Shock / fatigue | 4.0~5.0 | High-frequency cycling, shock loading |
| # | Common error | Consequence | Correct practice |
|---|---|---|---|
| 1 | Applying a formula without first deciding thin wall or thick wall | Using the thin-wall formula for a thick-wall cylinder gives a wall that is too thin | Decide D/δ first, then choose the formula |
| 2 | Taking the safety factor too small | Insufficient wall thickness with a risk of bursting | Static ≥ 2.5, dynamic ≥ 3 |
| 3 | Forgetting the fatigue check | Cracking under pulsating pressure | Raise n to 4 for high-frequency cycling |
| 4 | Using the wrong material strength | Treating cast steel as quenched and tempered steel gives a falsely high strength | Select σs by the grade in GB/T 8713 |
| 5 | Not checking the cylinder head connection strength | The thread or flange fractures and the cylinder head flies off | Check the cylinder head thread and flange at the same time |