Relative machinability rating and countermeasures of materials, for process planning and tool selection.
| Material | Machinability rating (45 steel = 1) | Main problem | Countermeasure |
|---|---|---|---|
| Aluminum alloy / brass | 3~5 (very easy) | Built-up edge, rough surface | Large rake angle, high speed, kerosene cooling |
| Gray cast iron | 1.5~2 (good) | Brittle chips, dust | Dry cutting or air cooling, wear-resistant insert |
| 45/40Cr quenched and tempered | 1 (baseline) | — | Conventional coated carbide |
| Q235 mild steel | 1~1.2 | Built-up edge, hard to break chips | Large rake angle + chip breaker, reduce speed appropriately |
| 304/316 stainless steel | 0.4~0.6 (difficult) | Work hardening, built-up edge, poor heat conduction | Low speed, large depth of cut, avoid small-feed rubbing, internal coolant tool |
| 42CrMo quenched and tempered (HB250+) | 0.6~0.8 | Fast tool wear | High-toughness insert, reduce Vc by 20% |
| Titanium alloy TC4 | 0.2~0.3 (very difficult) | Extremely poor heat conduction, flammable chips | Low speed, abundant internal coolant, avoid stopping the tool |
| Hardened part HRC50+ | 0.1 (very difficult) | — | CBN turning or grinding |
Stainless steel "work hardening" is the number-one pitfall: the cutting edge sliding in the hardened layer = chipping; feed must be maintained so the tool cuts into fresh metal. Use the accompanying cutting-parameter calculator (formula + recommended-range version) for cutting-parameter ranges.
See all quick calculators on the knowledge base home page.
Data compiled from publicly available GB/T standard tables for design reference only. For final design and acceptance, always consult the original standard and the latest supplier catalog.