Chemical composition per GB/T 3620 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| Ti | ≥99.0 (base) |
| Fe | ≤0.30 |
| O | ≤0.25 (interstitial control) |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Annealed | ≈440~620 | ≈275~430 | ≥18 | ≈120~180HV |
Used in annealed condition.
Heat exchangers, chlor-alkali equipment linings, seawater systems, medical instruments. No.1 among all metals in chloride-corrosion resistance.
TC4 titanium alloy (Ti-6Al-4V) AISI 304 stainless steel