Chemical composition per GB/T 1220 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | 0.11~0.17 |
| Cr | 16.0~18.0 |
| Ni | 1.50~2.50 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Quenched & tempered | 930~1080 (approx.) | 735~885 (approx.) | ≥12 | ≤285HB (Q&T) |
Oil quench around 1000°C, temper at 275~350°C (high-strength condition) or 550~650°C (toughness condition).
High-strength corrosion-resistant shafts, valve stems, pump shafts, marine fasteners. One of the highest-strength martensitic stainless grades.
AISI 420 (GB 2Cr13) martensitic stainless steel AISI 304 stainless steel