Worm gearing is not like an ordinary gear drive — the worm wheel material is soft (bronze) and the dominant failure modes are tooth flank scuffing, pitting and wear rather than broken teeth. Strength verification therefore focuses on the worm wheel, and the core is a double check of the tooth flank contact fatigue strength and the root bending fatigue strength. Below we work through an example of a 3 kW worm gearbox and then expand into the formulas.
A worm gearbox with input power P₁ = 3 kW, worm speed n₁ = 960 r/min and a gear ratio i = 30. The worm has z₁ = 2 starts, the worm wheel has z₂ = 60 teeth, the module is m = 5 mm, the worm pitch diameter is d₁ = 50 mm and the center distance is a = 175 mm. The worm wheel material is ZCuSn10P1 (tin bronze, sand cast) and the worm material is C45 steel surface hardened (>45HRC). Verify the tooth flank contact strength and the root bending strength of the worm wheel.
Worm torque:
Transmission efficiency (with z₁=2) η ≈ 0.78, worm wheel torque:
Worm wheel speed n₂ = n₁ / i = 960 / 30 = 32 r/min.
Lead angle:
cos γ = 0.9806, sliding velocity:
From the table (ZCuSn10P1 sand cast, worm hardness >45HRC, v_s ≈ 2.5 m/s):
| Parameter | Symbol | Value |
|---|---|---|
| Permissible contact stress | [σ_H] | 190 MPa |
| Permissible bending stress | [σ_F] | 50 MPa |
Worm wheel pitch diameter d₂ = m × z₂ = 5 × 60 = 300 mm. Load factor K = 1.1 (steady duty condition).
Parameter values: elastic coefficient Z_E = 155 √MPa (steel–tin bronze); contact coefficient Z_ρ = 3.1 (from the table for d₁/a = 50/175 = 0.286).
182.1 MPa < [σ_H] = 190 MPa ✅ the contact strength is acceptable
Equivalent tooth count:
From the table the tooth form factor is Y_F₂ = 2.0 (z_v₂ ≈ 64).
31.4 MPa < [σ_F] = 50 MPa ✅ the bending strength is acceptable
| Verification item | Calculated value | Permissible value | Conclusion |
|---|---|---|---|
| Tooth flank contact fatigue strength | 182.1 MPa | 190 MPa | ✅ Acceptable |
| Tooth root bending fatigue strength | 31.4 MPa | 50 MPa | ✅ Acceptable (large margin) |
Failures in worm gearing occur mainly on the worm wheel, because the worm wheel material (bronze) is far softer than the worm (steel). The common failure modes are:
| Material | Casting method | [σ_H] (MPa) | [σ_F] (MPa) | Application scenario |
|---|---|---|---|---|
| ZCuSn10P1 | Sand casting | 180~200 | 50 | High speed and heavy load, v_s < 12 m/s |
| ZCuSn10P1 | Centrifugal casting | 220~250 | 70 | High speed and heavy load, better performance |
| ZCuAl10Fe3 | Sand casting | 120~150 | 80 | Low speed and heavy load, v_s < 4 m/s |
| HT200/HT300 | Cast iron | 80~100 | 40 | Low speed and light load, v_s < 2 m/s |
Worm wheel torque:
Sliding velocity:
d₁ — worm pitch diameter; n₁ — worm speed; γ — lead angle
Tooth flank contact fatigue strength check:
| Parameter | Meaning | Typical value |
|---|---|---|
| Z_E | Material elastic coefficient | 155 √MPa (steel–tin bronze) |
| Z_ρ | Contact coefficient (from table) | 2.6~3.5 (d₁/a = 0.2~0.4) |
| K | Load factor | 1.0~1.4 (steady → impact) |
| a | Center distance (mm) | Fixed by the design |
| T₂ | Worm wheel torque (N·mm) | Calculated from the power and efficiency |
Tooth root bending fatigue strength check:
Y_F₂ — the worm wheel tooth form factor, determined from the equivalent tooth count z_v₂ = z₂/cos³γ.
| Duty type | K_A | K_v | K_β | Overall K |
|---|---|---|---|---|
| Steady load (conveyor belt, fan) | 1.0 | 1.0 | 1.0 | 1.0~1.1 |
| Moderate impact (hoist, agitator) | 1.0~1.2 | 1.1 | 1.1 | 1.2~1.4 |
| Severe impact (crusher, punch press) | 1.2~1.5 | 1.2 | 1.2 | 1.5~2.0 |
| Worm starts z₁ | Ratio range | Efficiency η | Lead angle γ | Application scenario |
|---|---|---|---|---|
| 1 | i > 30 | 0.70~0.75 | 3°~6° | High ratios, self-locking required |
| 2 | i = 15~30 | 0.75~0.82 | 8°~14° | Common choice, balancing efficiency and ratio |
| 4 | i = 8~15 | 0.82~0.88 | 14°~20° | Power transmission, efficiency first |
| No. | Common mistake | Consequence | Correct practice |
|---|---|---|---|
| 1 | Using 189 for the steel–steel elastic coefficient instead of 155 for steel–bronze | The contact stress comes out 16% too small and the design may actually be unsafe | Check the material pairing in the table; for steel–tin bronze take 155 |
| 2 | An error in the sliding velocity leads to the wrong permissible stress table row | A one-step error (180 vs 200 MPa) can reverse the verification conclusion | Compute the lead angle first and then the sliding velocity, and be accurate |
| 3 | Taking K = 1.0 without considering impact | The contact stress exceeds the limit under impact duty and pitting appears early | Select K from the table according to the characteristics of the prime mover and the driven machine |
| 4 | Omitting cos³γ in the equivalent tooth count | z_v₂ comes out too large → the tooth form factor is taken too small → the bending stress is underestimated | z_v₂ = z₂ / cos³γ, and the larger the lead angle the greater the effect |
| 5 | Verifying only the worm wheel and forgetting the worm shaft strength and stiffness | The worm twists too much and the mesh accuracy is affected | The worm shaft needs a separate combined bending and torsional strength check and a stiffness check |