Welding Groove Selection Quick Reference (Butt / Corner x Plate Thickness x Method)

Groove type recommended by joint form, plate thickness and welding method, used with weld symbols and welding material tables.

Joint typePlate thickness t (mm)Recommended grooveWelding methodPrecautions
Butt joint0.5~3Type I (no bevel)TIG / manual weldingDouble-side weld or back gouging
Butt joint3~6Single-V (60 deg)Manual arc / CO2Gap 1-2 mm, root face 1-2
Butt joint6~20Single-V / double-VSubmerged arc weldingUse X-type for thick plate to save material
Butt joint20~40Double-X (double side)Submerged arc weldingReduce distortion, symmetric welding
Butt joint40~60U-type / V-typeSubmerged arc + manualU-type saves filler metal
Butt joint>60Double-USubmerged arc weldingDeep groove needs preheating
Corner joint0.5~3Fillet weld (no bevel)Manual / CO2Leg length >= thin plate thickness
Corner joint3~10Single-bevelCO2Leg length by load
Corner joint10~30Double-bevel (symmetric)Submerged arcReduce angular distortion
T-joint0.5~3Fillet weldManual weldingDouble-side fillet weld
T-joint3~12Single-bevelCO2Bevel for good penetration
T-joint12~40Double-bevelSubmerged arcSymmetric to reduce distortion
Lap joint0.5~3Plug weld / spot weldCO2Lap width >= 3x thickness
Lap joint3~12Fillet/plug weldManual weldingIntermittent weld for long seams
Pipe butt joint2~6Type I (thin wall)TIGFull penetration
Pipe butt joint6~16Single-VTIG / manualBack shielding
Pipe butt joint16~40U-typeTIG + manualMulti-layer multi-pass
Flat surfacing—FlatSurfacingPreheat to prevent cracking
Heavy-plate vertical weld10~30V/X typeManual weldingBottom-up
Thin plate (stainless steel)0.5~2Type ITIGAnti-distortion fixture
Aluminium butt joint3~8Single-VTIGClean oxide film
Aluminium butt joint8~20Double-XTIGFront/reverse welding
Cast steel repair weld—U-typeManual weldingPreheat 150-300 deg C
Wear-resistant surfacing—Flat / toothedSubmerged arcSelect welding wire
Tack weld—Spot weldCO2Remove before final welding

Notes & calculation basis

Thin plate no bevel; medium-thick plate V-type, thick plate X/U-type to save filler metal and reduce distortion; groove angle, root face and gap shall be determined by procedure qualification. Stainless steel/aluminium need corresponding shielding gas.

Online calculators

See all quick calculators on the knowledge base home page.

Data compiled from publicly available GB/T standard tables for design reference only. For final design and acceptance, always consult the original standard and the latest supplier catalog.