Chemical composition per GB/T 1348 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | approx. 3.5~3.9 |
| Si | approx. 2.5~3.0 |
| Mn | ≤0.5 |
| Mg(res) | 0.03~0.06 (nodularizing) |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Separately cast test block | ≥450 | ≥310 | ≥10 | approx. 160~210HB |
As-cast or annealed (ferritic matrix, high plasticity).
Valve bodies, pipe fittings, housings, and shock-loaded bases. Plasticity close to low-carbon steel; weldability poorer than gray iron but still usable.
Ductile iron QT600-3 (EN-GJS-600-3) Gray cast iron HT200 (EN-GJL-200)