Chemical composition per GB/T 1220 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | ≤0.08 |
| Cr | 18.0~20.0 |
| Ni | 8.0~10.5 |
| Mn | ≤2.0 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Solution-treated | ≥520 | ≥205 | ≥40 | ≤187HB |
Solution-treated (rapid cooling from 1010~1150°C) as delivered. Pronounced work hardening; cannot be hardened by heat treatment.
Food/chemical equipment, piping, fasteners, and decorative parts. The most common stainless steel, synonymous with "stainless."
AISI 316 stainless steel AISI 201 stainless steel AISI 420 (GB 2Cr13) martensitic stainless steel