Chemical composition per GB/T 700 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | ≤0.22 |
| Si | ≤0.35 |
| Mn | ≤1.40 |
| P/S | ≤0.045/0.045 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Hot-rolled (Grade A, ≤16mm) | 370~500 | ≥235 | ≥26 | approx. 120~140HB |
Generally supplied and used in the hot-rolled condition without heat treatment. Normalizing (around 900°C, air cooling) may be applied to improve the microstructure.
Welded structural members, sections, plates, bolts, frames, guardrails, and non-critical load-bearing parts. It is the most widely used general-purpose structural steel.
Q355B low-alloy high-strength steel (GB) C45 (AISI 1045) carbon steel 08F rimmed carbon steel (GB)