Chemical composition per GB/T 3190 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| Al | ≥99.6 |
| impurities | Fe/Si mainly |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| O temper | ≥60 | ≥15 | — | approx. 20~25HB |
| H14 temper | approx. 100 | ≥90 | — | approx. 30HB |
Not heat-treatable for strengthening; strength raised by cold working (H temper).
Nameplates, rating plates, conductive busbars, chemical-vessel linings, and reflector hoods. Lowest strength but best corrosion resistance + electrical/thermal conductivity.
AA5052 aluminium-magnesium alloy (GB) AA6061-T6 aluminium alloy