MOULDLKnowledge Base3D Model DownloadsMembership
中文版Model Store »
Knowledge Base › Standard Data › Common Heat-Treatment Processes and Hard
HomeModels
Table of contents

Knowledge Base Home

📐 Standard Data

🧮 Calculators

📖 Selection Guides

🏭 Material Grades

❓ Engineer FAQ

🗂 Quick-Reference Categories

❌ Error Case Studies

📚 Technical Articles

Common Heat-Treatment Processes and Hardness Ranges

Hardness and depth achievable by quenching/tempering, carburizing, nitriding, induction; reference for drawing call-outs.

ProcessApplicable materialHardness rangeCase depthFeature
Normalizing45/35/ZGHB 170~229ThroughImproves machinability, uniform structure
Quenched and tempered45/40Cr/42CrMoHB 200-300 (adjustable)ThroughBalanced mechanical properties; most common
Quench + mid-temp temper45/65MnHRC 42~50ThroughSprings, wear parts
Surface hardening (induction/flame)45/40CrHRC 45-58 (core quenched & tempered)1~2 mmGear flanks, journal surfaces
Carburizing + quench20Cr/20CrMnTiTooth flank HRC 58-620.5~1.5 mmLow-carbon steel; hard surface, tough core
Nitriding (gas/plasma)38CrMoAl/42CrMo≥550 HV0.3~0.5 mmMinimal distortion, wear & corrosion resistant

Notes & calculation basis

Nitriding must be preceded by quenching-and-tempering; carburized-quenched parts must be ground (leave grind allowance). Example call-out 'Quenched & tempered 220-250 HB' is far more inspectable than 'heat treated'.

Online calculators

See all quick calculators on the knowledge base home page.

Data compiled from publicly available GB/T standard tables for design reference only. For final design and acceptance, always consult the original standard and the latest supplier catalog.

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL