Heat Treatment Process / Hardness / Applicable Part Reference

Reference of common heat treatment process names, achieved hardness and typical applicable parts, for process route planning and hardness requirement marking.

Process nameCode / standardAchieved hardnessApplicable partsPurpose / notes
Annealing (full)GB/T 16922≤HB229Forgings / castingsStress relief, softening
NormalizingGB/T 16922HB170~230Carbon steel forgingsRefine structure
Quenching (C45 steel)GB/T 16924HRC50~55Shafts / gearsIncrease hardness
Quenching and tempering (quench + high-temp temper)GB/T 16924HB200~350Connecting rods / boltsStrengthen and toughen
Surface hardening (induction)GB/T 16923HRC45~58Journal / tooth flankHard surface, tough core
CarburizingGB/T 9450HV550-700 (case)Gears / camsImprove wear resistance
NitridingGB/T 18177HV600-900 (case)Precision partsHigh hardness, corrosion resistant
CarbonitridingGB/T 18177HV500~700Small partsWear-resistant, anti-scuffing
Low-temp tempering150~250℃HRC55~60Tools / gaugesRelieve quenching stress
Medium-temp tempering350~500℃HRC35~50Springs / forging diesElasticity / toughness
High-temp tempering500~650℃HB200~350Quenched and tempered partsStrength and toughness
Stress-relief annealing500~650℃—Welded partsRelieve residual stress
Spheroidizing annealingGB/T 16922HB170~210Tool steelImprove machinability
Isothermal annealing—HB170~220Alloy steelPrevent flake (white spot)
Artificial aging100~200℃Slight increaseCastings / aluminiumRelieve internal stress
Bluing / blackening—Decorative / rust-proofStandard partsSurface oxidation
Galvanizing (zinc plating)——Outdoor partsCathodic protection
Hard chrome plating—HV800~1000Plungers / moldsWear resistance
Soft nitriding—HV500~700MoldsReduce friction
Laser quenching—HRC55~62Local strengtheningLow distortion
Vacuum quenching—HRC58~62Precision partsNo oxidation
Temper brittleness prevention——Cr-Ni steelFast cool, avoid 450 deg C
Boronizing—HV1200~1500MoldsHigh wear resistance
Shot peening—Compressive stress layerSprings / gearsImprove fatigue
Phosphating——Steel / ironRust-proof / friction reduction
Quench crack control———Control cooling / preheating
Annealing (ductile iron)GB/T 16922HB180~230Ductile iron partsGraphitization
Solution treatment (stainless steel)GB/T 13305—Austenitic stainlessPrevent intergranular corrosion
Hydrogen removal treatment200~300℃—Plated partsPrevent hydrogen embrittlement
Normalizing + temperingGB/T 16922HB180~250Cast steel partsStabilize structure

Notes & calculation basis

Hardness is a typical range, actually depending on material and process; quenching and tempering = quench + high-temp temper, surface hardening/carburizing/nitriding for "hard surface, tough core"; heat treatment distortion and cracking see material heat treatment FAQ.

Online calculators

See all quick calculators on the knowledge base home page.

Data compiled from publicly available GB/T standard tables for design reference only. For final design and acceptance, always consult the original standard and the latest supplier catalog.