Chemical composition per GB/T 1173 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| Si | 6.5~7.5 |
| Mg | 0.30~0.50 |
| Ti | 0.08~0.20 |
| Al | Balance |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| T6 metal-mold cast | 280~320 (approx.) | — | — | 80~100HB (approx.) |
T6: solution (535°C) + artificial aging (150°C). Modification refines eutectic silicon.
Complex housings, pump bodies, brackets by sand/permanent-mold casting. ≈ ASTM A357.
Cast aluminium alloy ZL104 (Al-Si9Mg, ASTM A360) AA6061-T6 aluminium alloy