Chemical composition per GB/T 1220 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | 0.16~0.25 |
| Cr | 12.0~14.0 |
| Ni | ≤0.60 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Q&T | ≥635 | ≥440 | ≥20 | approx. 192~223HB |
| Quenched + low-temp tempered | — | — | — | approx. 48~52HRC |
Oil quench at 1000~1050°C, hardness set by tempering temperature: low-temp temper gives high hardness, high-temp temper at 600~700°C gives good toughness.
Parts needing rust resistance plus hardenability: pump shafts, valve stems, cutting tools, surgical instruments, and corrosion-resistant bolts.