Chemical composition per GB/T 1220 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | ≤0.08 |
| Cr | 17.0~19.0 |
| Ni | 9.0~12.0 |
| Ti | 5×C~0.70 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Solution-treated | ≥520 | ≥205 | ≥40 | ≤187HB |
Solution treatment + stabilization (850~900°C). Ti fixes carbon to prevent intergranular corrosion.
Chemical piping/equipment that cannot be solution-treated after welding, and corrosion-resistant parts serving at 450~800°C.