MIG/MAG/TIG wire and shielding-gas pairing (plus electrode matching) for welding process cards.
| Base material | Welding wire | Shielding gas | Remarks |
|---|---|---|---|
| Mild steel Q235/45 | ER50-6(H08Mn2SiA) | CO₂ or Ar80%+CO₂20% | Mixed gas gives less spatter and better bead |
| Low-alloy high-strength steel Q355 | ER50-6/ER55-G | Ar+CO₂ mixed gas | For critical structures choose over-matching |
| 304 stainless steel | ER308/ER308L | Pure Ar (TIG)/Ar+2%CO₂ (MAG) | L = low carbon, resists intergranular corrosion |
| 316 stainless steel | ER316L | Same as above | — |
| Aluminum alloy 5/6 series | ER5356 / ER4043 | Pure Ar | 5356 higher strength, 4043 better crack resistance |
| Submerged-arc welding mild steel | H08A + welding flux HJ431 | — | Long straight thick-plate butt joints |
Equal-strength matching is the principle: the deposited-metal strength of the wire only needs to meet ≥ the lower limit of the base-metal standard; no over-matching (over-matching cracks instead). Stainless wires containing L (low carbon) are for intergranular-corrosion-resistant applications. Shielding gas flow 10~20 L/min; add a wind shield in windy conditions.
See all quick calculators on the knowledge base home page.
Data compiled from publicly available GB/T standard tables for design reference only. For final design and acceptance, always consult the original standard and the latest supplier catalog.