Chemical composition per GB/T 3077 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | 0.32~0.40 |
| Si | 1.10~1.40 |
| Mn | 1.10~1.40 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Quenched & tempered (25mm test bar) | ≥885 | ≥735 | ≥15 | 207~269HB (approx.) |
Q&T: oil quench at 850~880°C, temper at 520~570°C.
Common on older drawings: shafts, gears, worms. A classic substitute for 40Cr.
41Cr4 (AISI 5140) alloy steel GB 40MnB boron alloy structural steel (AISI 15B41)