Chemical composition per GB/T 3191 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| Mg | 0.8~1.2 |
| Si | 0.4~0.8 |
| Cu | 0.15~0.40 |
| Cr | 0.04~0.35 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| T6 temper | approx. 290~310 | approx. 240~270 | approx. 10 | approx. 95HB |
Solution (530°C water quench) + artificial aging (175°C × 8 h) = T6. Profile mills deliver T6 directly.
Equipment frames, jigs and fixtures, machined parts, and profiles. The default choice for mechanically structured aluminium.
AA6063-T5 aluminium alloy AA7075-T6 aluminium alloy AA5052 aluminium-magnesium alloy (GB)