Typical strength and density of 2A12/6061/6063/7075/5052 for lightweight structural material selection.
| Grade / temper | Tensile sigma_b (MPa) >= | Yield sigma_s (MPa) >= | Density (g/cm3) | Typical use |
|---|---|---|---|---|
| 2A12-T4 (LY12) | 425 | 275 | 2.78 | High-strength structures, aircraft frames |
| 6061-T6 | 310 | 276 | 2.70 | General sections, fixtures, equipment frames |
| 6063-T5 | 160 | 110 | 2.69 | Decorative sections, heatsinks, conveyor extrusions |
| 7075-T6 | 560 | 500 | 2.81 | Ultra-high strength: dies, high-load structures |
| 5052-H32 | 215 | 160 | 2.68 | Sheet metal, fuel tanks, corrosion-resistant panels |
Aluminum alloys have a high yield-to-tensile ratio and no clear fatigue limit plateau; weld HAZ strength drops 30-50% (6061 needs re-aging after welding). 7075 resists seawater poorly. The T5/T6 difference for extrusions lies in cooling and aging process.
See all quick calculators on the knowledge base home page.
Data compiled from publicly available GB/T standard tables for design reference only. For final design and acceptance, always consult the original standard and the latest supplier catalog.