Chemical composition per GB/T 1591 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | ≤0.20 |
| Si | ≤0.50 |
| Mn | 0.90~1.65 |
| P/S | ≤0.035 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Hot-rolled (≤16mm) | 470~630 | ≥355 | ≥21 | approx. 135~160HB |
Used in the hot-rolled or normalized condition; thick plates may be normalized to improve toughness and reduce anisotropy.
Welded structures, bridge girders, booms, large frames, and construction-machinery structural parts. About 50% stronger than Q235 while retaining good weldability.
Q235 carbon structural steel (GB) C45 (AISI 1045) carbon steel