Chemical composition per GB/T 2965 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| Al | 5.5~6.8 |
| V | 3.5~4.5 |
| Ti | balance |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Annealed | ≥895 | ≥825 | ≥10 | ≈30~36HRC |
Annealing: air cool at 700–800°C. Cannot be strengthened by conventional quenching (α+β type; solution + aging used for specific parts).
Aerospace structures, medical implants, high-strength corrosion-resistant chemical parts, racing / bicycle components. The champion of specific strength.