Chemical composition per GB/T 699 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | 0.05~0.11 |
| Si | ≤0.03 |
| Mn | 0.25~0.50 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Cold-rolled annealed | ≥295 | ≥175 | ≥35 | ≤131HB |
Usually used in the cold-rolled annealed condition; carburizing and quenching can be applied after stamping to increase hardness.
Deep-drawn parts, automotive body panels, gaskets, and drawn housings. Excellent plasticity with very low strength.
AISI 1020 carbon steel (GB 20) Q235 carbon structural steel (GB)