Chemical composition per GB/T 3077 standard range (reliability: high); mechanical properties are typical values / ranges (reliability: medium) — acceptance is governed by the purchase standard and the mill test certificate.
| C | 0.12~0.18 |
| Cr | 0.80~1.10 |
| Mo | 0.40~0.55 |
| Condition | Tensile MPa | Yield MPa | Elong. % | Hardness |
|---|---|---|---|---|
| Normalized + tempered | ≥440 | ≥295 | ≥22 | ≈135~165HB |
Normalizing: air cool around 900°C; tempering: 650°C. Good weldability (vs. medium-carbon alloy steel).
Steam pipes, boiler heating-surface tubes, heat-resistant parts ≤550°C. A classic steel in power / boiler industry.
30CrMo alloy structural steel (quenched and tempered)