E41-371 · Guide Rail Selection · Humid-Environment Rail Base Rust · ★★★
During the southern plum-rain season (90% humidity), rust bulges appeared on the cast-iron guide rail mounting base, about 2~5mm in diameter, lifting the rail about 0.02mm at the bulge.
The guide rail mounting base is cast iron (HT300), finished without rust protection. Under the sustained high humidity of the plum-rain season (90%RH), the cast iron surface underwent electrochemical corrosion. Graphite (C) in the iron acts as the cathode and ferrite as the anode, forming micro-cells that oxidize iron to Fe₂O₃·nH₂O (rust). Rust expands about 6× in volume (Fe→Fe₂O₃), forming bulges on the base surface. The bulges are about 0.02mm high and 2~5mm in diameter. The rail mounted on the bulged base was lifted locally, and straightness degraded from 0.005mm/m to 0.025mm/m. As sliders passed the bulge, resistance increased and chatter marks appeared on the machined surface.
① Immediately apply anti-rust oil to the rail base after finish machining (thickness ≥0.01mm)\n② Upgrade base material: cast iron → chrome-plated cast iron or stainless-steel cladding\n③ Control workshop environment: humidity ≤70% (add dehumidifiers)\n④ Inspect the base for rust before rail installation (dress rust spots with an oilstone)\n⑤ Apply anti-rust primer to the base during installation (epoxy zinc-rich primer, salt-spray resistance ≥500h)
FT_10_Linear Guideway Selection