E41-026 · Bearing Selection · Mine Crusher Vibrating Screen · ★★★★
After about 1 month the bearing noise increased markedly and vibration worsened; disassembly showed the raceway packed with mineral and dust, the grease black and muddy. The cage was severely worn and the rolling elements showed abrasive wear.
An open bearing with a Z-type metal shield (non-contact seal, about 0.3mm gap) was used. Around the mine crusher the dust concentration is very high (respirable dust ≥10mg/m³); ore powder is mostly 10~50μm, some below 5μm. A 0.3mm gap cannot block such fine dust. The screen's strong vibration (amplitude 8mm, frequency 16Hz) acts as a pump, actively drawing dust into the bearing. The quartz in the dust has hardness HV≈1000, exceeding bearing steel's HV≈700, and directly abrades the raceway.
① Per ISO 12944 environment classification: mines are C5-I (high corrosion, high dust) or CX
② Seal upgrade: choose a double-sided contact rubber seal (2RS) bearing
③ 2RS seal: nitrile rubber lip slides on the inner ring at 0.5~1N/mm contact pressure, dust block rate >99%
④ Add external auxiliary seal: labyrinth seal at both housing ends (3~5 ring grooves + grease fill)
⑤ Positive-pressure air seal: feed 0.05MPa compressed air into the labyrinth, continuously exhausting outward to block dust
⑥ Periodic maintenance: re-grease every 500h (purge old contaminated grease via relief port)
FT_23_Bearing Selection Specification