E41-132 · Bearing Selection · Rolling-Mill Bearing Housing · ★★★★
After the rolling-mill bearing housing's bearing failed, only a new bearing was fitted, but it overheated and failed again within 2 weeks. Disassembly showed the outer ring rotating in the bore (outer-ring creep/walk).
During service the housing bore wore from outer-ring fretting, growing from Φ280H7 (+0~+0.052mm) to Φ280.15mm (a 0.1mm increase). The worn bore was not measured when fitting the new bearing—it was installed directly. The Φ280mm outer-ring fit went from interference to clearance (about 0.1mm gap). Under rolling force F_r=500kN the outer ring could not be held in the bore and rotated relative to it (creep/walk), accelerating wear and generating high heat. Wear debris from the rotating ring also entered the lube system, speeding bearing wear. The correct approach is to restore the bore to original size before installing the new bearing.
① A worn housing bore must be repaired: sleeve / brush-plating / spraying then re-bore
② Bore roundness and size inspection: mandatory each time it is disassembled
③ After repair bore tolerance Φ280H7 (+0.052/0), surface roughness Ra≤1.6μm
④ Apply bearing retaining compound (Loctite 641) at installation for extra hold
⑤ Keep a housing bore size record, logged each bearing change
FT_23_Bearing Selection Specification