E41-543 · Bearing Selection · Hammering Force Denting the Bearing Raceway · ★★★
When the bearing was installed the hammering force was transmitted through the cage to the rolling elements and produced 0.002mm dents on the raceway surface, which later spalled in service.
When pressing the bearing onto the journal, the operator hammered the outer ring with a copper bar (an incorrect operation), so the hammering force passed from the outer ring through the rolling elements into the inner ring raceway. The hammering force on a single rolling element is F_impact≈10000N (the impact of a hand hammer), and the contact stress between the rolling element and the inner ring raceway is σ_H=0.388×√(10000×206000²/5²)≈3200MPa (R = 2.5mm the raceway curvature radius). The material yield strength is about 2000MPa and 3200MPa > 2000MPa, so the raceway surface develops plastic deformation (denting) about 0.002mm deep. Although the dent is shallow, the raised edge (about 0.001mm) produces stress concentration as the rolling elements pass, and after about 10⁴ cycles fatigue cracks initiate at the edge of the dent and propagate into spalling.
1) Bearing installation force must never be transmitted through the outer ring (the rolling elements);
2) The installation force must act directly on the tight ring of the fit (pressing the shaft → pressing the inner ring end face);
3) Use a press (hydraulic or screw press) for installation;
4) Use heated installation (oil bath 80~100℃, so the bearing slides into place without stress);
5) After installation, measure the bearing rotation torque (it should be no more than 20% above normal).
FT_23_Bearing Selection Standards