E41-587 · Bearing Selection · Precision Rolling Mill Bearing Housing Ovality · ★★★★
After machining, the rolling mill housing bore had an ovality of 0.03mm (requirement ≤0.01mm). The bearing turned stiffly once fitted and after two weeks of running the bearing heated up (75℃).
The housing bore (Φ200H7, tolerance +0~+0.046mm) was bored on a boring machine and finished with an ovality of 0.03mm. When the outer ring of the four-row taper roller bearing is fitted into an oval bore the outer ring is squeezed along the major axis and has clearance along the minor axis. The outer ring distortion Δd≈0.03mm reduces the internal radial clearance of the bearing by about 0.02mm along the major axis and increases it by 0.01mm along the minor axis. The load distribution over the four rows of rollers becomes severely uneven: the load on the two rows along the major axis increases (about 40% more) while the load on the two rows along the minor axis falls. The contact stress in the most heavily loaded row of rollers rises from 1200MPa to about 1700MPa, 94% of the contact fatigue limit of the bearing steel (about 1800MPa). In service that row of rollers heats up (up to 85℃), the grease thins and is lost, further accelerating the wear. After about two weeks the raceway of that row of rollers began to spall and the bearing temperature continued to rise.
1) Housing bore machining accuracy: roundness ≤0.008mm (precision grade ≤0.005mm);
2) Housing bore inspection: measure three sections with an inside micrometer, four directions per section;
3) An out-of-tolerance ovality can be repaired by lapping or by re-machining after plating;
4) After fitting the bearing, check the rotation torque (it should be uniform with no local jamming);
5) For large bores, prefer turning on a lathe (a boring machine tends to produce ovality because of the tool overhang).
FT_Bearing Design Handbook