E41-138 · Reducer Coupling Selection · Press Pneumatic Clutch · ★★★★
The press pneumatic clutch smokes during continuous stamping; friction-disc temperature reaches 350 ℃ and the friction material burns and breaks. Disassembly shows the disc is completely carbonized.
The press clutch's original friction discs are copper-based powder metallurgy (temperature rating 400 ℃, friction coefficient 0.35); during replacement, resin-based friction material (rating 250 ℃, coefficient 0.4) was mistakenly used. The press stamps 60 times per minute; each engagement slip-friction work W = ½Jω² = 0.5×2.5×31.4² ≈ 1232 J. Per-minute slip work W_total = 1232×60 = 73920 J/min ≈ 1.23 kW. The resin-based material's allowable continuous slip power is ~0.3 kW (no forced cooling), but actual 1.23 kW is 4× over. The friction-surface temperature quickly rises to 350 ℃, exceeding the resin material's limit (250 ℃); the resin carbonizes and fails, and the disc breaks. Copper-based powder metallurgy has an allowable continuous slip power of ~1.5 kW and runs normally under this duty.
① The clutch friction disc must use the OEM-specified material (copper-based powder metallurgy)
② Never substitute powder metallurgy with resin-based friction material (different temperature ratings)
③ Slip-work check: W ≤ W_permitted × 1.2 (safety factor)
④ Install a temperature sensor on the clutch (alarm above 200 ℃)
⑤ Run break-in after disc replacement (first 100 engagements at half load)
FT_13_Reducer-Motor Matching Selection