E41-253 · Reducer Coupling Selection · Reducer Housing Casting Defect · ★★★
After 1 week of operation a new reducer shows a crack at the housing joint face with oil leakage; crack length ~30 mm, located on the bearing-bore side wall.
The reducer housing is an HT250 cast-iron part; at the bearing-bore side wall there is a shrinkage-porosity defect from casting (shrinkage cavity, ~2 mm diameter, ~3 mm deep). The local wall thickness is only 10 mm, and the porosity reduces effective thickness ~30%. Under combined bearing preload and gear-mesh force, the stress-concentration factor near the porosity is Kt ≈ 4, local stress σ_peak = Kt×σ_nom = 4×15 = 60 MPa, exceeding HT250's fatigue limit (~40 MPa). After 1 week (~10⁴ cycles) a fatigue crack initiates at the porosity and grows through the wall thickness, finally penetrating to form an oil-leak path.
① Critical cast areas (bearing bore / joint face) should get X-ray inspection\n② Improve casting process: add riser + chill to eliminate shrinkage porosity\n③ Wall-thickness design: bearing-bore side wall ≥15 mm (more safety margin)\n④ After machining do an air-tightness test (0.3 MPa air + soapy-water check)\n⑤ After finding a crack, repair weld: open a V-groove → weld with nickel-based electrode → stress-relief heat treatment
FT_13_Reducer-Motor Matching Selection