E41-266 · Cylinder and Hydraulic Selection · Aged-Cylinder Seal Groove · ★★★
A hydraulic cylinder used for 5 years lost thrust from 80 kN to 50 kN, with large speed fluctuations. Disassembly inspection found about 0.2 mm wear at the bottom of the piston seal groove, so the seal could no longer seal effectively.
The hydraulic cylinder piston seal (V-type combination seal) is installed in a groove of 5 mm depth. During 5 years of service, the seal undergoes high-frequency micro-motion in the groove (the seal receives a tangential force at each piston reversal), and the groove bottom and sidewalls suffer fretting wear of about 0.2 mm. In the deepened groove the seal's contact pressure against the cylinder bore wall drops, reducing sealing effectiveness. High-pressure oil enters the low-pressure chamber through the clearance between seal and bore; the internal leakage Q_leak ≈ 20 L/min (at 20 MPa) equals about 15% of pump flow. The effective thrust F_eff = F_theory×(1 − Q_leak/Q_pump) = 80×(1 − 0.15) = 68 kN, but the measured value is 50 kN (also including friction losses).
① Repair if seal-groove wear exceeds limit (>0.1 mm): build up by welding then re-machine groove\n② Or replace piston (new piston machined to standard seal-groove dimensions)\n③ Change seal from V-type to U-type (U-type seal adapts better to groove wear)\n④ Use seal material with anti-wear additive (PTFE + bronze powder, groove wear reduced 50%)\n⑤ Periodically check cylinder internal leakage (pressure-hold test every 1000 h)
FT_32_Hydraulic System Design