E41-439 · Sensor Electrical Selection · Welding-Fume Laser-Sensor Contamination · ★★★
After 1 month at a welding station, the laser displacement sensor's readings drifted about 0.5mm, returning to normal after lens cleaning. A white fume deposit coated the lens surface.
Welding fumes generated during welding (mainly metal oxides Fe₂O₃/MnO₂, particle size 0.1~1μm) disperse in air and deposit on the laser sensor lens surface. Within 1 month the deposit thickness reaches about 0.02mm. The deposit reduces laser transmittance from 90% to about 30% (67% intensity attenuation). The reflected-light intensity the laser sensor receives is insufficient; the internal algorithm auto-gain-compensates, but the compensated signal SNR drops and the reading drifts about 0.5mm. In addition, metal-oxide particles in the deposit scatter the laser (stray light), further interfering with measurement. After lens cleaning, intensity recovers and the reading returns to normal.
① Add an air curtain to the laser sensor at the welding station (continuous compressed-air lens purge, pressure 0.1MPa, flow 50L/min)\n② Or add a protective cover + quartz glass window (replace glass periodically, avoiding direct lens contamination)\n③ Clean the lens periodically (lint-free cloth + isopropanol each shift)\n④ Sensor mounting distance ≥2m (away from the welding-fume source)\n⑤ Use a large-spot laser sensor (spot diameter >0.5mm, insensitive to surface contamination)
FT_33_Sensor Selection Guide