Knowledge Base › Selection Error Cases › Galvanic corrosion between a steel pipe fitting and a copper pipe causing leakage (cooling water system)

Galvanic corrosion between a steel pipe fitting and a copper pipe causing leakage (cooling water system)

E41-153 · Other Selection · Cooling Water System Pipe Fitting · ★★★

Problem Description

The joint between the copper pipe and the steel pipe fitting began leaking after 6 months of service; on teardown the steel fitting threads were heavily rusted and the copper pipe end had also corroded and thinned.

Root Cause

A copper pipe (T2 pure copper) was connected directly to a steel pipe fitting (45 steel, galvanized), forming a galvanic corrosion cell in the electrolyte of the water (cooling water containing about 50mg/L Cl⁻). The standard potential of copper is +0.34V and that of steel is -0.44V, giving a potential difference ΔE=0.78V. In the cooling water the steel acts as the anode and undergoes oxidation (Fe→Fe²⁺+2e⁻), with a corrosion rate V_corr=K×ΔE/(ρ×A) ≈ 0.5mm/year. After 6 months the corrosion depth on the steel fitting threads reached about 0.25mm; the thread strength dropped and the seal failed. The corrosion product Fe₂O₃ (rust) expands in volume about 6 times and blocked the sealing face, but the loose rust cannot seal, so the cooling water seeped out through the corroded gap. Meanwhile dissolved copper ions (Cu²⁺) deposited on the steel surface, causing secondary corrosion.

Corrective Solution

① Galvanic corrosion protection is required wherever dissimilar metals make contact
② Option A: change the steel fitting to nickel plating (nickel potential -0.25V, only 0.59V difference from copper)
③ Option B: switch to a brass pipe fitting (brass H62 potential -0.13V, 0.47V difference from the copper pipe)
④ Option C: fit an insulating gasket (nylon or PTFE, completely isolating the dissimilar metals)
⑤ Add a corrosion inhibitor to the water (molybdate / phosphate, which forms a protective film on the metal surface)

Checklist

Reference

FT_Machine Design Handbook