Knowledge Base › Selection Error Cases › Worn tapered-pin locating hole leading to loss of locating accuracy (fixture locating)

Worn tapered-pin locating hole leading to loss of locating accuracy (fixture locating)

E41-298 · Other Selection · Fixture Tapered-Pin Locating · ★★★

Problem Description

After one year of use, the tapered-pin locating hole of a machining-center fixture degraded in locating accuracy from ±0.01mm to ±0.05mm. The pin hole became elliptical.

Root Cause

The fixture locating uses a Φ10mm tapered pin (1:50 taper), with a hardened-steel locating bushing (HRC58~60). During workpiece clamping and removal, the tapered pin is subjected to impact and friction in the locating bushing. About 500 load/unload cycles per week amount to about 26000 per year. Under repeated impact, the bushing surface suffers fretting wear, with a wear depth of about 0.02mm. After wear, the bushing bore enlarges, and the pin's locating taper can no longer fully contact the bore (only the less-worn areas make contact), reducing the effective contact area by about 50% and lowering locating accuracy. In addition, the guiding action of the tapered pin in the bushing weakens with each insertion (fit clearance increasing from 0.005mm to 0.025mm), further worsening the locating error.

Corrective Solution

① Upgrade the locating bushing material: hardened steel→cemented carbide (wear resistance increased 10 times)\n② Replace the locating bushing after wear (spare-parts management, replace every six months)\n③ Switch to cylindrical pin + expansion sleeve locating (an alternative to the tapered pin)\n④ Automatic lubrication of the locating pin (micro oil-mist lubrication to reduce wear)\n⑤ Increase the surface hardness of the tapered pin (carburized and hardened HRC60→titanium coating HV2000)

Checklist

Reference

FT_Machine Design Handbook

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »