E41-459 · Other Selection · Stainless Steel Pipe Intergranular Corrosion · ★★★★
A 304 stainless steel pipe developed cracks 3 months after welding (along the weld heat-affected zone) and leaked. Metallographic analysis revealed grain-boundary corrosion (intergranular corrosion) in the heat-affected zone.
During welding of 304 stainless steel, the weld heat-affected zone (HAZ, temperature range about 500~850℃) undergoes sensitization. In this temperature range, chromium at the grain boundaries combines with carbon to form Cr₂₃C₆ carbides that precipitate along the grain boundaries, dropping the chromium content near the grain boundaries from 18% to about 10% (below the minimum 12% required for corrosion resistance). In a chemical medium containing Cl⁻ (about 50ppm), intergranular corrosion occurs in the chromium-depleted zone and propagates along the grain boundaries, forming intergranular cracks. After 3 months the cracks penetrated the pipe wall (3mm thick), causing leakage. The weld was not solution-treated (heating the pipe to 1050℃ and then rapidly cooling it to redissolve the carbides).
① When welding 304 stainless steel, use the low-carbon grade (304L, C≤0.03%, not easily sensitized)\n② Or use a stabilized stainless steel (321/Ti or 347/Nb, where the added Ti/Nb preferentially forms carbides)\n③ Perform solution treatment after welding (1050℃×10min + water cooling, eliminating sensitization)\n④ Control the Cl⁻ concentration of the medium (≤10ppm to reduce the corrosion rate)\n⑤ Subject the weld to an intergranular corrosion test (sulfuric acid-copper sulfate method, ASTM A262E)
FT_Machine Design Handbook