E41-791 · Other Selection · Secondary Grouting Crack · ★★★
The secondary grout layer between the equipment base and foundation (design thickness 50 mm, actual 20 mm) developed cracks and spalling after 3 months of operation.
The secondary grout layer was only 20 mm thick, below the minimum recommended 30 mm (required by the grout manufacturer). During hardening, the thin-layer grout develops shrinkage stress σ_s = E×ε = 25×10⁹×0.0005 = 12.5 MPa (E = 25 GPa elastic modulus of grout, ε = 0.05% shrinkage). This 12.5 MPa shrinkage stress exceeds the grout's tensile strength (about 4 MPa), producing microcracks inside the layer (width about 0.02 mm). Operating vibration of the equipment (velocity 4 mm/s) propagates the cracks → spalling → debonding of the grout layer from the base → loss of support → deformation of the equipment base → destruction of coupling alignment.
① Recheck all parameters per correct selection specifications
② Confirm that operating loads, environment, and service life all meet design requirements
③ Select reliable brands and appropriate models
④ Verify installation and operating conditions
⑤ Perform periodic inspection and maintenance after commissioning