Knowledge Base › Selection Error Cases › Tooth-surface thermal cracks caused by insufficient gear lubrication and cooling (continuous-duty gear)

Tooth-surface thermal cracks caused by insufficient gear lubrication and cooling (continuous-duty gear)

E41-621 · Gear Transmission Selection · Continuous-duty Gear Lubrication · ★★★★

Problem Description

A continuously operating gearbox (running 24 h/day) developed a network of thermal cracks (crazing) on the tooth surfaces after 8 months, with crack depths of 0.1~0.3 mm, appearing as a crazed pattern.

Root Cause

During long-term continuous operation, the flash temperature in the mesh zone of the gear tooth surfaces accumulated and caused tooth-surface thermal fatigue. The lubricating oil was VG320 mineral oil with an oil temperature of 65℃ (at the bearing end). The pitch-line velocity of the gear was 15 m/s, giving a calculated flash temperature T_flash≈120℃, so the tooth-surface temperature = oil temperature 65℃ + flash temperature 120℃ = 185℃. Mineral oil oxidizes rapidly at 185℃ (the oxidation rate doubles for every 10℃ rise; the 185/65 difference of 120℃ → 2¹²=4096 times), so the oil oxidized and deteriorated after 1~2 months, with the acid value rising from 0.5 to 3.0 mgKOH/g. The acidic oil corroded the tooth surface, producing stress-corrosion cracks under contact stress. Meanwhile, the tooth surface underwent one thermal cycle per mesh (room temperature → 185℃ → room temperature × 24 h × 240 days = about 1.38 million thermal cycles); the thermal stress σ_th=E×α×ΔT=206000×12×10⁻⁶×160≈395 MPa (linear expansion coefficient of carbon steel 12×10⁻⁶/℃, temperature difference 185-25=160℃). 395 MPa is close to the yield strength of the gear material (40Cr quenched and tempered) of 450 MPa, and the tooth-surface layer, under the combined repeated thermal and mechanical stress, developed fatigue cracks that propagated in a crazed pattern.

Corrective Solution

① The lubricating oil for continuously operating gears must be a synthetic oil (PAO, with an oxidation-resistant life 5~10 times longer than mineral oil)\n② Increase the cooling oil flow (raise the jet flow rate from 2 L/min to 5 L/min to lower the tooth-surface temperature)\n③ Fit an oil cooler to the gearbox (to keep the oil temperature ≤55℃)\n④ Apply a protective coating to the tooth surface (copper plating 0.01 mm, to prevent corrosion and reduce friction)\n⑤ Test the lubricating oil regularly (check the acid value and viscosity monthly; replace immediately if out of limits)

Checklist

Reference

FT_Gear Transmission Design

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »