Knowledge Base › Selection Error Cases › Early tooth-surface failure caused by grinding burn of the hardened case (gear grinding process)

Early tooth-surface failure caused by grinding burn of the hardened case (gear grinding process)

E41-623 · Gear Transmission Selection · Gear Grinding Process Problems · ★★★★

Problem Description

After 50 h of bench testing, the ground gear (20CrMnTi carburized and hardened to HRC60) showed grinding-burn marks (temper bands) on the tooth surface, with the hardness dropping to HRC48~52.

Root Cause

During gear grinding the grinding depth was too large (ap=0.05 mm per pass, recommended ≤0.02 mm per pass), with a grinding wheel (corundum, grain size 60) linear speed of 35 m/s. The grinding heat Q=P/v_cut=1000/35≈28.6 J/mm (tangential force P about 1000 N/mm ÷? incorrect estimate). The instantaneous temperature in the actual grinding zone can reach 300~500℃ (depending on cooling conditions). The cooling effect of the grinding fluid is blocked by an air-film layer during high-speed grinding (the air boundary layer on the wheel surface prevents the coolant from reaching the contact zone), so the actual cooling efficiency is only 20~30%. The 300~500℃ exceeds the tempering temperature of the carburized case (200℃), causing high-temperature tempering of the carburized case (martensite decomposing into tempered sorbite), with the hardness dropping from HRC60 to HRC48~52 to a depth of about 0.1 mm. The meshing tooth surface with reduced hardness underwent plastic deformation under a contact stress of 850 MPa, developing wear pits 0.05~0.1 mm deep after about 50 h (normal wear resulting from insufficient surface hardness, not fatigue pitting).

Corrective Solution

① Gear grinding process parameters: rough grinding ap≤0.03 mm per pass, finish grinding ap≤0.01 mm per pass\n② Wheel selection: use a CBN wheel (high thermal conductivity, 80% less grinding heat) instead of a corundum wheel\n③ Coolant: high-flow, high-pressure jet (pressure ≥1 MPa, flow ≥30 L/min)\n④ After grinding, check by nital etching (temper burn appears black; re-hardening burn appears white)\n⑤ Check the hardness after grinding (the tooth-surface hardness must not be less than 95% of the carburized-and-hardened hardness)

Checklist

Reference

FT_Gear Transmission Design

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL