E41-640 · Gear Drive Selection · Gear Inventory Corrosion · ★★★
A large spare gear (m = 16 mm, ZG35CrMo, tooth-surface hardened) was installed and put into use after 2 years in storage; after 1 month of operation, pitting appeared on the tooth surface, and inspection revealed corrosion micro-pits.
During storage the gear was not coated with rust-preventive oil (only ordinary machine oil) and was kept in an open-air warehouse (relative humidity > 80%), so the hardened tooth-surface layer (HRC50) corroded in the damp environment. The corrosion pits were 0.05–0.1 mm deep (pitting) and 0.5–2 mm in diameter. No tooth-surface inspection was done before installation (visual only, and visual inspection can hardly find corrosion micro-pits). After operation, the tooth-surface contact stress was σ_H = 700 MPa; stress concentration occurred at the corrosion pits (Kt ≈ 3), giving a local stress σ_H_peak ≈ 2100 MPa, exceeding the tooth-surface contact fatigue limit (about 1200 MPa). Micro-cracks formed at the edges of the corrosion pits → propagated → formed pitting (5–10× the original corrosion pits). After about 1 month, more than 20 pits appeared on the tooth surface and the gear failed.
① Gear spares must be coated with rust-preventive oil (protection period ≥ 2 years) and sealed in packaging\n② Storage environment: temperature 15–25 °C, humidity ≤ 60%, no corrosive gases\n③ A tooth-surface visual inspection must be performed before installation (with a 10× magnifier or dye penetrant testing)\n④ Gears stored longer than 1 year should have their accuracy and surface condition re-inspected before installation\n⑤ Inspect the rust-prevention condition of stock gears every 6 months and re-coat with oil
FT_Gear Transmission Design