E41-861 · Belt Drive Selection · Cold-Storage Conveying · ★★
On a cold-storage (-25℃) conveyor the belt hardened at low temperature and slipped on start-up, so it had to be barred over by hand every shift to help it start, sharply cutting efficiency.
First, ordinary rubber has a glass-transition temperature Tg ≈ -20℃, and -25℃ is already below Tg; the elastic modulus E rose 5× and the belt hardened and lost its elasticity. Second, the increased hardness lowered μ from 0.3 to 0.15 and halved F_f = F0·μ·e^(μα) → at a starting torque T_s = 2T, F_e exceeded F_f and the belt slipped. Third, the hardened belt saw a higher bending stress σ_b and tended to break on cold start-up. [Root cause] The low-temperature rating was insufficient.
① Below < -20℃ a cold-resistant belt must be used (CR neoprene rated to -40℃, or silicone rubber rated to -60℃)
② State the minimum ambient temperature in the selection and choose the material by its Tg
③ Add insulation/local heating in the cold-storage area to keep the belt zone > -20℃
④ Use a soft starter to clip the starting peak
⑤ Set the tension at the upper limit to compensate for the drop in μ
⑥ Do not use an ordinary rubber belt below < -20℃
⑦ Check belt hardness and cracks every shift