Knowledge Base › Selection Error Cases › Link-plate fatigue fracture caused by excessive chain tension (scraper conveyor)

Link-plate fatigue fracture caused by excessive chain tension (scraper conveyor)

E41-656 · Chain Drive Selection · Scraper Conveyor Chain Fracture · ★★★★

Problem Description

After three months of operation, the link plates of a scraper-conveyor chain (24A, double-strand) broke in batches at the pin holes; teardown revealed that the link plates were blued, showing the color of high-temperature tempering.

Root Cause

The chain tension was adjusted too high: the actual tension F_tension = 8 kN (4–5 kN recommended).

Corrective Solution

The excessive tension brought the bearing stress at the pin hole close to the allowable limit. Under hydrogen embrittlement and high stress the link plate underwent delayed fracture.
① Chain tension should be 1–2% of the chain's own weight
② Link-plate tempering temperature 420–450 ℃ (HRC35–40 is optimal)
③ Dehydrogenation treatment is mandatory after phosphating
④ Enlarge the transition fillet at the link-plate pin hole
⑤ Perform hardness and tensile spot checks on each batch of link plates

Checklist

Reference

FT_Belt & Chain Drive Design

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL