Knowledge Base › Selection Error Cases › Brittle fracture of a chain at low temperature (cold store)

Brittle fracture of a chain at low temperature (cold store)

E41-967 · Chain Drive Selection · Cold-Store Chain Drive · ★★

Problem Description

In a cold store at -25℃ a plain chain fractured brittly and dropped parts.

Root Cause

First, plain chain steel loses notch toughness at low temperature and fractures brittly under impact. Second, -25℃ raises notch sensitivity and the chain breaks. Third, parts dropped. [Root cause] Insufficient low-temperature resistance.

Corrective Solution

① For low temperatures use a low-temperature steel chain (Ni steel / quenched and tempered for toughness)
② Specify the minimum temperature in the selection
③ Add insulation to reduce cooling
④ Do not use a plain chain at deep-low temperature
⑤ Periodically check for brittleness
⑥ Avoid impact loads
⑦ On break, check temperature

Checklist

Reference

FT_Belt & Chain Drive Design