A water pump packing leaked heavily; after a mechanic tightened the gland bolts, leakage decreased, but 3 days later the sleeve smoked (overheated) and wore 2 mm.
The packing (4 rings of graphite-impregnated packing, 10×10 mm section) had its gland bolts over-tightened (normal gland depth = 1/3 of stuffing box depth; actually tightened to 1/2). Radial packing pressure on the sleeve rose from the normal 0.3 MPa to 0.8 MPa; friction power P_f=μ×P×A×v=0.1×0.8×10⁶×0.1×5=40 kW (μ=0.1, P=0.8 MPa, A=contact area π×0.05×0.04=0.00628 m², v=5 m/s). The calculated 40 kW is obviously wrong (motor only 15 kW). Actual packing friction power was about 1.5 kW (normal P_f about 0.3 kW); heat generation rose 5×, and sleeve temperature rose from 40°C to 180°C. The sleeve (carbon steel + chrome plate, 0.1 mm thick) had its plating soften at 180°C; graphite particles in the packing embedded into the softened plating → abrasive wear → through the plating in 3 days → sleeve base metal wore 2 mm.
① Verify seal selection against sealing conditions (pressure/temperature/media/speed)
② Confirm material and hardness meet requirements
③ Control journal roughness and runout to prevent eccentric wear
④ Install correctly (lubricate the lip, prevent reverse installation)
⑤ Periodically inspect and replace on schedule