High-Pressure O-Ring Extrusion (Ultra-High-Pressure Jack)

E41-901 · Seal Component Selection · Ultra-High-Pressure Jack · ★★★★

Problem Description

One 70 MPa jack's O-ring had no backup ring; it was extruded into a 0.2 mm gap and sheared, pressure dropped and load capacity fell.

Root Cause

First, critical extrusion clearance g_c drops with pressure; at 70 MPa g_c≈0.03 mm, but here 0.2 mm>>g_c. Second, the ring is extruded and shear τ exceeds its shear strength. Third, pressure drop loses load and wastes labor. Root cause: high pressure without backup ring + large clearance.

Corrective Solution

① Ultra-high pressure (>30 MPa) O-rings must have backup rings + clearance ≤0.03 mm
② Backup rings of high-strength PTFE/PEEK on the low-pressure side
③ Select high-hardness rings (Shore 90)
④ Verify g_c vs. pressure curve
⑤ Do not run high pressure with large clearance and no backup ring
⑥ Check backup rings for shear damage each time
⑦ If load drops, check extrusion immediately

Checklist

Reference

FT_Seal Spring Design