E42-458 · Fatigue Fracture · High-Speed Rail Bogie Frame · ★★★
Bogie welded frame weld seam crack 25mm long; speed-restricted operation; 1 train repaired per month
[Weld Seam Stress] Operating dynamic load σa=90MPa, R=-0.3, near S-N limit.
[Fatigue] Hot spot stress concentration.
[Design Omission] Weld seam not ground; operating speed not limited; safety factor 1.4 (should be ≥2.0).
1) Grind weld seam smooth;
2) Bond FRP patch at hot spot;
3) Limit operating speed;
4) Upgrade material to S355;
5) Flaw detect each train;
6) Reduce dynamic load;
7) Thicken web plate;
8) Periodic re-measurement.
GB/T 25343-2010