Knowledge Base › Structural Design Error Case Study › Induction-Hardening Transition Zone Causing Soft-Band Spalling

Induction-Hardening Transition Zone Causing Soft-Band Spalling

E42-227 · Heat Treatment Distortion and Cracking · Camshaft · ★★★

Problem Description

Soft band between the hardened zone and core spalls, wearing fast.

Root Cause

[Transition Soft Band] Uneven induction scanning speed leaves a 3mm soft band at the end of the hardened zone. [Spalling Wear] The soft band is low in strength and spalls by contact fatigue. [Design Omission] No overlap zone, hardening parameters fluctuate.

Corrective Solution

1. Provide an overlap zone ≥10mm on the inductor.
2. Keep scanning speed steady on the hardening machine.
3. Use closed-loop power control for parameters.
4. Low-temperature temper after hardening.
5. Hardness gradient inspection.
6. Sample soft bands each batch.
7. Finish-grind the cam profile.
8. Fully spray coolant.

Checklist

Reference

GB/T 9451-2005

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL